Machine design
Screw and barrel: diameter, compression and wear
The screw is the part of the machine that turns resin into a parison, and the part most often blamed for problems it did not cause. What diameter, compression and wear actually change.
Diameter sets output, not quality
Plasticising capacity scales roughly with the square of screw diameter for the same screw design and speed. A jump from 65 mm to 80 mm is about 1.5 times the output, which is why the screw is chosen from the heaviest container at the required cycle, not from the container volume.
| Diameter | Typical plasticising rate | Fits |
|---|---|---|
| 45–50 mm | 25–38 kg/h | Small bottles, multi-cavity |
| 55–65 mm | 48–60 kg/h | 1 L to 3 L bottles |
| 70–75 mm | 75–90 kg/h | 4 L to 6 L containers |
| 80–95 mm | 95–140 kg/h | 10 L to 12 L containers |
| 100–120 mm | 150–210 kg/h | 20 L to 25 L drums |
Compression ratio and why it matters
Compression ratio is the flight depth at the feed end divided by the depth at the metering end. A general-purpose screw for HDPE and PP sits around 2:1 to 3:1. Too low and the melt is not compacted; too high and the shear generates heat you cannot remove.
Materials with a narrow processing window — PVC, PETG — use lower compression and a longer metering section. This is why one screw cannot be optimal for every material, even when it can run all of them.
Wear: the failure that hides
Barrel and screw wear does not announce itself. Output slowly drops, the cycle stretches, and the operator compensates by raising temperature — which makes the problem worse.
| Symptom | What it suggests |
|---|---|
| Output falls over months at the same settings | Flight or barrel wear |
| Melt temperature has to be raised to keep the same quality | Increased clearance, more shear |
| Black specks that return after purging | Carbon in a worn flight root |
| Surge in output | Uneven wear or a chipped flight |
Wear comes from filled compounds, abrasive pigments, glass-filled regrind, and running dry. Nitrided barrels handle unfilled resin; filled material needs a bimetallic barrel.
Replace or rebuild
Measure the barrel bore and the flight outside diameter against the original drawing. If clearance has grown beyond about 0.3–0.5 mm depending on size, output and quality will not come back by adjustment. A nitrided screw can sometimes be re-sleeved or re-nitrided; a bimetallic barrel is usually replaced, not rebuilt.
Where to go next
- KSY model range — screw sizes and plasticising rates
- Output calculation — the plasticising check in formula three
- Maintenance schedule — what to check and when
- HDPE or PP — why the screw design differs by material
Need a machine sized for your container?
Send the container size, weight, material and the output you need. We answer with a machine proposal and a capacity calculation, not a catalogue.