PVC in extrusion blow molding: where it still wins

PVC is the material most processors try to avoid and a few still run every day, because nothing else gives the same glass-clear wall with a soft squeeze. Here is what it demands from the machine, and where it no longer pays.

Why PVC still earns its place

Rigid PVC, with no plasticiser added, does three things at once that are hard to buy together. It is genuinely clear: a 1 mm wall passes close to 88% of visible light, with a faint blue edge that reads as glass rather than plastic. It resists alcohols, oils, dilute acids and aliphatic hydrocarbons. And it creeps instead of cracking, so a squeeze bottle dents and recovers without stress whitening at the shoulder.

That is why PVC still holds shampoo, bath gel, clear household cleaners and edible oil, where the label has to show the product through the wall.

The screw and die head PVC needs

PVC will not run on a general-purpose polyethylene screw. It is shear-sensitive and sits close to its degradation temperature at ordinary conditions, so the screw must be gentle and the flow path clean.

  • Dedicated screw, 20:1 to 24:1 L/D, compression ratio 2.0–2.5:1, gradual transition and deep metering flights. A barrier screw built for HDPE will scorch the material in the transition zone.
  • Bimetallic barrel liner and a chrome-plated, streamlined die head. Hydrogen chloride attacks steel, and a corroded channel puts black specks into the next batch.
  • Low screw speed, 20–40 rpm, with melt at 175–190 °C. Anything above 200 °C at the die is a countdown, not a setpoint.
  • Residence time under 6–8 minutes, and a die with no threaded plugs or sudden expansions where material can sit and cook.

Heat history is the whole game

PVC degrades by splitting off hydrogen chloride, and the HCl then catalyses further degradation. Shear, iron and time all accelerate it. The first sign is rarely a black streak; it is a color shift, white going cream and cream going amber.

  • Never stop the screw with PVC at temperature for more than a few minutes.
  • Purge with polyethylene or a commercial purging compound before every shutdown.
  • Keep a separate granulator and regrind box; a handful of PVC flake contaminates a PET or HDPE stream.
  • No brass or copper scrapers in the flow path, because both catalyse degradation.

Regrind is usable at 10–15%, and only from parts that were never overheated. Recycling discolored scrap simply concentrates the problem.

Where it loses

PETG took most clear cosmetic work away from PVC for good reasons: no chlorine, no HCl corrosion, a wider processing window and better gloss straight off the mold. It brings drying and lower melt strength with it, but a plant running both usually keeps PETG on the shared machine and PVC on a dedicated one.

HDPE wins wherever the bottle does not need to be clear. It is tougher, far better against surfactants in stress crack tests, needs no corrosion protection and causes no argument at the recycler. Above roughly 500 ml, detergent and household chemical bottles are HDPE by default.

The PVC niche left is narrow but real: a clear, chemically resistant, squeezable bottle in small to medium sizes, on a line that runs PVC often enough to justify its own screw, die head and purge discipline.

Property PVC PETG HDPE
Clarity Clear, faint blue edge Clear, bright gloss Translucent at best
Chemical resistance Oils, alcohols, dilute acids; poor against ketones and aromatics Moderate; attacked by chlorinated solvents and strong alkalis Acids, alkalis, surfactants; poor against hydrocarbons
Squeeze feel Soft, holds a dent, recovers Stiffer, springs back Stiff, whitens when dented
Processing window Narrow, 175–190 °C Moderate, requires drying Wide and forgiving
Machine demand Dedicated screw, corrosion protection, purge routine Dryer, low-shear screw General-purpose screw
Recycling Chlorine contaminant, falling acceptance Polyester stream, growing Established stream