Extrusion blow molding machines, molds and line equipment for 5 ml bottles to 25 L jerry cans

KESYER KSY blow molding machinery

Tooling

Blow pin and neck finish: the interface that decides whether a bottle leaks

The neck is the only part of a blow molded container with a tolerance that matters to the filling line. Most leaks, capping problems and customer complaints trace back to it — and to the blow pin that formed it.

What the blow pin does

The blow pin enters the parison, seals against the inside of the neck, passes air into the container, and forms or calibrates the bore. It is a wear part in a precision role, which is a bad combination: it wears slowly, so the drift is invisible until the capping line complains.

Type Used for Note
Standard blow pin Most containers Calibrates the bore; air passes through the pin
Blow pin with cutter Containers needing a clean top edge Trims the neck in the mold
Needle blow Small openings, handles Leaves a small mark that must be sealed or hidden

The four things that go wrong at the neck

  1. Insert cooling. The neck is the thickest section relative to its surface. Without its own cooling circuit in beryllium copper, it stays soft and distorts on ejection.
  2. Pin wear. A worn pin gives a bore that is out of round or oversized; caps then leak or spin.
  3. Misalignment. A pin that is not concentric with the neck insert shaves one side of the bore and leaves a witness mark.
  4. Clamp force. Too little and the neck moves during blow; too much and the insert is stressed.

How to check, cheaply

  • Go/no-go gauges on the bore and the thread, on the first five containers after every mold change.
  • Visual check for a witness line or shaving on the bore.
  • Cap torque test on a sample, if the filling line has a capper.
  • Cavity number marked on the mold, so a defect can be traced to one cavity.

Two minutes of gauging at the machine is cheaper than a pallet of leaking bottles at the customer.

When to replace a blow pin

Not on a calendar. Replace when the bore gauge shows drift, when the bore shows a mark from the pin, or when the cap torque test fails. Keep one spare pin per cavity in stock: a pin is inexpensive relative to the downtime of waiting for one.

Where to go next

Need a machine sized for your container?

Send the container size, weight, material and the output you need. We answer with a machine proposal and a capacity calculation, not a catalogue.

Send your container