MATERIALS
Barrier basics: EVOH, nylon and what each one actually stops
A barrier layer is a promise about shelf life. Before choosing between EVOH and nylon, decide what you are keeping out of the bottle, or keeping in it, because the two resins are not interchangeable.
What a barrier has to stop
Four transport problems drive almost every barrier project. Oxygen gets in and oxidises edible oil, juice and sauces. Carbon dioxide gets out of anything carbonated. Solvent and hydrocarbon permeate through the wall of an agrochemical or fuel container, which is a safety issue as much as a shelf-life one. Moisture moves in both directions, but HDPE already handles that on its own.
The numbers put the gap in perspective. Dry EVOH is roughly two orders of magnitude better than HDPE against oxygen. Nylon sits between the two, and its barrier recovers once the resin dries out again.
EVOH: excellent, but only while dry
EVOH is a copolymer whose ethylene content sets the trade-off. Lower ethylene gives a better oxygen barrier and worse moisture tolerance; 32 mol% is the usual blow molding grade, with 44 mol% chosen when humidity is the bigger problem.
The material absorbs moisture, and a wet EVOH layer loses most of its oxygen barrier. That single fact explains the whole layer structure: the EVOH has to be buried between polyolefin skins, with tie layers to bond it.
- Five layers: HDPE / tie / EVOH / tie / HDPE. EVOH at 2–5% of wall thickness, typically 20–50 µm, with 10–20 µm of tie on each side.
- Six layers add a regrind layer: HDPE / regrind / tie / EVOH / tie / HDPE. Keep EVOH out of that regrind or the scrap comes back as gels.
- Dry the EVOH before running, around 60–65 °C, and keep it sealed between shifts.
Nylon: the chemical barrier
PA6, PA66, MXD6 and the amorphous nylons are chosen for hydrocarbons and solvents rather than for oxygen. They resist fuels, many agrochemical actives and aromatic solvents that would pass through HDPE in weeks.
The cost is process temperature. Nylon runs at 240–260 °C, so the polyethylene skins have to tolerate the heat and the tie layer has to survive it too. MXD6 bonds more readily to PE than PA6 does, which is why it appears so often in fuel and solvent containers.
Nylon also takes up moisture and loses barrier when wet, but unlike EVOH it recovers on drying, so a wet test result is not necessarily a formulation failure.
Surface treatment and the alternatives
Fluorination and sulfonation treat the inside of an HDPE bottle instead of adding a layer. They are simpler than coextrusion and need no tie layers, but the barrier is thin, easily scratched and carries its own regulatory questions for food contact. Oxygen scavengers work differently again: they are active, finite and consumed over the shelf life, where a multilayer barrier is passive and lasts as long as the wall does.
| Barrier | Best against | Weak against | Moisture | Typical layer |
|---|---|---|---|---|
| EVOH 32 mol% | Oxygen, CO2, odours | Moisture, some solvents | Highly sensitive | 20–50 µm |
| EVOH 44 mol% | Oxygen in humid conditions | Still moisture limited | Moderately sensitive | 20–50 µm |
| PA6 | Hydrocarbons, solvents | Oxygen, moisture | Recovers on drying | 30–80 µm |
| MXD6 | Hydrocarbons, CO2 | Oxygen | Recovers on drying | 30–80 µm |
| HDPE | Moisture | Oxygen, CO2, solvents | Unaffected | Whole wall |
| Fluorination | Solvents, hydrocarbons | Oxygen, scratching | Unaffected | Surface only |
Check layer thickness on a cross-section, not on the drawing, and pull a peel test at the shoulder where the layers stretch most. Delamination shows up first as white streaks at the neck.
Where to go next
- Multilayer blow molding machine — the hardware side of three, five and six layer structures.
- When three layers pays — the economics of adding layers before you commit to them.
- Chemical containers — solvent and agrochemical packs where nylon earns its place.
- Multilayer jerry can line — a worked example of a barrier structure in production.
- Food and milk bottles — where oxygen and light, not solvents, set the requirement.
Need a machine sized for your container?