Extrusion blow molding machines, molds and line equipment for 5 ml bottles to 25 L jerry cans

KESYER KSY blow molding machinery

Applications

Blow molding machines for lubricant oil bottles

1 L, 4 L and 5 L engine oil bottles with handles and view stripes, and 18 – 20 L lubricant cans.

1 L to 5 L engine oil bottles

Containers

Engine oil and lubricant packaging

Oil bottles are mostly rectangular with handles and offset necks, often with a view stripe. They need even corner walls and clean handle deflashing.

  • 1 L engine oil bottles on 4 or 6 cavities
  • 4 L and 5 L bottles with handles
  • Bottles with transparent view stripes
  • 18 L and 20 L lubricant cans

Engineering

What makes a lubricant bottle hard

A lubricant bottle looks simple: a squat body, a wide neck, a handle on the larger sizes, a screw cap. What makes it difficult is that it carries 4 to 5 kg of liquid, it is sold by the case, and it is stacked. The container has to be light enough to compete on resin cost and strong enough to survive a pallet falling over.

The handle is the first problem. Above 3 L almost every lubricant bottle is handled, and the handle is formed by pinching the parison, which stretches the wall at exactly the point where the load concentrates. A handle root at 0.8 mm will pass a drop test empty and fail it full, because the mass of the oil multiplies the stress. Handle designers talk about the root as a beam, not as a wall: it needs a minimum section and a radius, and it needs to be fed from a thick part of the parison.

The wide neck is the second. Lubricant bottles use 38 – 51 mm necks so the oil flows in quickly, and a wide neck means a large unsupported circle at the top of the parison. That is where ovality appears, and ovality is what makes a cap leak on one side only. The neck insert has to be cooled harder than the body, and the blow pin has to be concentric with it.

The third is the product itself. Oil attacks nothing in HDPE, but it does swell some regrind if the regrind has been contaminated, and it picks up odour from a barrel that was running something else. On a line that changes product, the purge discipline matters more than the machine settings.

Range

Container range and what it demands

ContainerTypical weightNeckWallWhat decides the design
500 ml – 1 L oil bottle28 – 45 g38 – 43 mm0.8 – 1.1 mmNeck squareness; label panel flatness
1 – 2 L with offset neck45 – 70 g38 – 45 mm0.9 – 1.2 mmNeck position; wall opposite the neck
3 – 4 L handled80 – 120 g43 – 48 mm1.0 – 1.4 mmHandle root; base corner
4 – 5 L handled110 – 170 g45 – 51 mm1.1 – 1.5 mmTop load in a two-high stack; handle beam
1 L with in-mould label45 – 60 g38 – 43 mm0.9 – 1.2 mmLabel placement in the cavity; static charge

Typical values for HDPE. A container that will be stacked three high needs the base and shoulder at the top of these ranges.

Selection

Choosing the machine by container size

Production cycles for HDPE, including extrusion, blow and cooling. Shot weight is the mass of one cycle.

ContainerModelDie heads × stationsShot weightCycleOutput per hour
500 ml – 1 L oil bottleKSY75-J6L3 × 2 = 60.17 – 0.27 kg28 – 34 s635 – 770
1 – 2 L offset neckKSY85-J10L2 × 2 = 40.18 – 0.28 kg26 – 34 s420 – 550
3 – 4 L handledKSY85-J10L1 × 2 = 20.16 – 0.24 kg30 – 38 s190 – 240
4 – 5 L handledKSY95-J12L1 × 2 = 20.22 – 0.34 kg34 – 44 s165 – 210
5 L, single stationKSY105-J15L1 × 1 = 10.11 – 0.17 kg30 – 40 s90 – 120

Output = 3,600 ÷ cycle × containers per cycle, calculated. The last row is for a 5 L container with a very heavy base or a mould too large for two stations.

A handled container is a heavier container at the same volume, and that is why a 4 L oil bottle runs on a 12 L platform rather than a 10 L one. The extra platen distance is what gives the handle room; the extra clamping force is what keeps the base from flashing.

Process

The process window

ParameterTypical settingWhat goes wrong outside it
Melt temperature185 – 205 °CAbove: sag in a heavy parison. Below: a rough surface on the label panel
Mould temperature, body10 – 16 °CWarm: longer cycle and a panel that bows after filling
Mould temperature, neck6 – 10 °CWarm: oval neck and a cap that leaks on one side
Blow pressure0.5 – 0.8 MPaLow: short base corners. High: flash string on the seam
Parison profile12 – 20 pointsFlat profile: thick shoulder, thin base corner
Handle pinchSharp land, 0.2 – 0.3 mmWorn: a web that has to be cut by hand

Quality

Tests that decide acceptance

TestWhat it provesWhere it typically fails
Corner drop, filledThe handle and base survive a fall from a palletHandle root and base corner
Top load, two or three highThe stack does not deform the shoulderShoulder ring and cap seat
Leak and cap torqueThe closure holds in transit and at temperatureNeck ovality
Weight by cavityAll cavities run the same wallOuter cavities on a wide head spacing
Oil resistance and swellingThe container does not soften after a month of contactRegrind-rich sections
Label adhesionThe wrap label sits flat after fillingPanel curvature

Troubleshooting

Defects and where they come from

What you seeUsual causeWhat to change first
Handle root cracks when fullRoot stretched from a thin parison sectionMove the handle to the parting line, thicken the root
Oval neck, cap leaks one sideNeck insert cooling too warm, or pin off centreDrop the neck circuit 3 °C, check concentricity
Flash ring under the neckPinch land wornResurface the land
Base corner thinParison too short, or profile pushing material upLengthen the parison, move profile points down
Panel bows after fillingEjected too hotExtend cooling, drop mould temperature 2 °C
Colour drift after a changeRegrind from the previous colour in the binSegregate regrind, purge the head

Line

Line configuration and a worked example

ItemSpecification for a 4 L oil bottle line
Blow molding machineKSY95-J12L, Ø90 mm screw, single die head, double station
MouldSingle cavity, hardened pinch land, neck insert on its own cooling circuit
De-flashingOne unit per station, cutting against the mould
Leak testingSample testing, or 100% if the cap is a tamper-evident type
ConveyorAccumulation before packing
Chiller and granulatorAir-cooled chiller; granulator returning flash at a fixed ratio

Worked example: a 4 L oil bottle at 130 g, two cavities, 38 s cycle. Shot weight is 2 × 0.13 = 0.26 kg, so the plasticising demand is 0.26 ÷ 38 s = 25 kg/h, well inside the 125 – 140 kg/h of the KSY95-J12L. Output is 3,600 ÷ 38 × 2 = 190 bottles an hour.

The machine is not the limit here; the mould is. A single cavity on a double station means the second station waits for the same parison, so the output is set by one mould half per cycle. Two cavities per station would double the output, but then the shot weight is 0.52 kg and the cycle has to stretch to about 44 s for cooling — which is where the real trade-off sits.

Evidence

From projects we have built

A 1 L bottle project in Indonesia runs 1 L containers on a 5 L platform, three cavities on a double station, to keep the handle wall and the cycle honest. 1 L bottles on a 5 L platform.

For the container family see chemical containers, and for the arithmetic how to calculate blow molding output.

Oil bottle line with robot take-out and labeling.

See the line

Oil bottles with robot take-out and labeling

A KSY75-J6L oil bottle line: the robot takes the bottles out of the mold and passes them on for labeling.

FAQ

Questions

Which machine for a 4 L or 5 L oil bottle?

KSY95-J12L for 4 – 5 L handled bottles, KSY85-J10L for 1 – 3 L. The handle, not the volume, decides the platform: the parison has to fill the handle and the body in the same cycle.

Why does the handle crack on a full bottle but not an empty one?

The handle root is the thinnest section of the container, and a full bottle multiplies the stress at exactly that point. The fix is to feed the root from a thicker part of the parison and move the handle to the parting line.

What neck size do oil bottles use?

Usually 38 – 51 mm, so the oil flows in quickly. A wide neck means a large unsupported circle at the top of the parison, which is why the neck insert needs its own cooling circuit.

Why does the cap leak on one side only?

The neck is oval, usually because the neck insert is too warm or the blow pin is not concentric. Check the pin first, then drop the neck circuit 3 °C.

Can you run in-mould labelling on an oil bottle?

Yes, with a mould that holds the label in the cavity and a controlled static charge. The label adds a few seconds to the cycle because the film has to be placed and held before the blow.

How much regrind in a coloured oil bottle?

20 – 30% on hidden parts. Colour drift is the limit, not strength: regrind from a previous colour shows on the shoulder first.

Do oil bottles need a barrier?

Normally no. HDPE resists mineral and synthetic oils well. Barrier is used where the product is a solvent or where odour loss matters, and that is a multilayer machine.

What decides the cycle on a thick-base oil bottle?

The base. A 1.5 mm base corner takes longer to freeze than the 1.0 mm body, and the container cannot be ejected until the base is solid, or it sinks in the pallet.

Get a quote

Send us your container

Send the drawing or a photo with volume, weight and material, and the output you need. We recommend the machine and mold.