Extrusion blow molding machines, molds and line equipment for 5 ml bottles to 25 L jerry cans

KESYER KSY blow molding machinery

Applications

Blow molding machines for cosmetic bottles

Lotion, toner, cream, hair care and sample bottles in PE, PP and PETG, from 5 ml to 1 L, on multi-cavity molds.

Extrusion blow molded cosmetic bottles

Containers

Cosmetic and personal care bottles

Cosmetic bottles change often and need a good surface. Extrusion blow molding makes many shapes with low mold cost, in opaque, translucent or clear materials.

  • Lotion and cream bottles with pumps
  • Toner and serum bottles in clear PETG
  • Hair care and shower gel bottles
  • Travel and sample bottles from 5 ml

Engineering

Why cosmetic bottles are a different problem

A cosmetic bottle is bought for how it looks, and everything else follows from that. The wall has to be clear enough to read a label through, the base has to be thick enough to feel like glass in the hand, the seam has to be invisible on the shelf, and the neck has to take a pump that clicks into place at a fixed height. None of these are strength requirements, and that changes which machine you need.

Clarity is a resin and temperature question before it is a machine question. PETG is the usual choice for glass-like clarity, and it is hygroscopic: moisture left in the pellet hydrolyses in the barrel and shows up as haze and a weak weld line. A dryer is not optional on a PETG line. Clarified PP gives a translucent bottle rather than a clear one, at a lower resin cost and a much wider process window.

The thick base is where the cycle goes. A 2 mm base on a 200 ml bottle needs three to four times the cooling of the 0.8 mm body, and the base is the last part to solidify because it is furthest from the mould wall. Cooling the base insert separately, in beryllium copper rather than steel, is what makes the difference between a 30-second cycle and a 45-second one.

Then there is the neck. Cosmetic packs use small pump and disc-top closures where the pump sits at a controlled height, so the neck has to be square and the bore concentric. A neck that is 0.2 mm out of square leaks at the collar, and the customer finds it on the filling line, not at the moulding machine.

Range

Container range and what it demands

Weights are typical for PETG; clarified PP runs 10 – 15% lighter for the same wall.

ContainerTypical weightNeckWall / baseWhat decides the design
5 – 30 ml sample or serum bottle6 – 14 g18 – 20 mm0.8 mm / 1.5 mmClarity; neck concentricity for the dropper
30 – 50 ml pump bottle14 – 24 g20 – 24 mm1.0 mm / 2.0 mmPump height; base weight in the hand
50 – 100 ml lotion bottle22 – 40 g24 mm1.0 – 1.3 mm / 2.0 mmSeam visibility; panel flatness
100 – 200 ml toner or shampoo35 – 65 g24 – 28 mm1.2 – 1.5 mm / 2.5 mmBase clarity; cooling time
200 – 500 ml body lotion60 – 110 g28 mm1.4 – 1.8 mm / 3.0 mmThick base without bubbles; cycle
PETG vs clarified PPPP −10 – 15%samesamePP: translucent, cheaper, wider window. PETG: clear, slower, needs drying

Selection

Choosing the machine by container size

The thick base is the reason these cycles are longer than a bottle of the same volume in HDPE. Shot weight is the mass of one cycle and is what the screw has to plasticise.

ContainerModelDie heads × stationsShot weightCycleOutput per hour
5 – 30 ml serum bottleKSY45-J1.8L4 × 2 = 80.05 – 0.11 kg18 – 24 s1,200 – 1,600
30 – 50 ml pump bottleKSY50-J2L4 × 2 = 80.11 – 0.19 kg22 – 28 s1,030 – 1,300
50 – 100 ml lotion bottleKSY50-J2L2 × 2 = 40.09 – 0.16 kg26 – 32 s450 – 550
100 – 200 ml toner bottleKSY55-J2.5L2 × 2 = 40.14 – 0.26 kg30 – 38 s380 – 480
200 – 500 ml body lotionKSY65-J3L1 × 2 = 20.12 – 0.22 kg36 – 46 s155 – 200

Output = 3,600 ÷ cycle × containers per cycle, calculated for PETG at the weights above. Clarified PP runs 10 – 20% faster because it does not need the same base cooling.

Note what happens between the 50 – 100 ml and the 200 – 500 ml rows: the number of cavities drops from four to two even though the containers are not that different. The reason is the base. A 3 mm base on a 300 ml bottle will not cool inside a 30-second cycle, and the only way to keep the cycle honest is to make fewer of them per cycle.

Process

PETG and clarified PP process windows

ParameterPETGClarified PP
Drying before processingRequired: 65 – 70 °C for 4 – 6 h, dew point −20 °C or lowerNot required
Melt temperature200 – 225 °C195 – 215 °C
Mould temperature8 – 14 °C15 – 25 °C
Base insert coolingSeparate circuit, beryllium copper insertSeparate circuit recommended
Blow pressure0.4 – 0.6 MPa0.4 – 0.6 MPa
RegrindDry before re-use; keep below 20% on visible partsUp to 30% on hidden parts

PETG punishes two things: moisture and dwell time. Wet resin gives haze and a weld line at the base; resin that sits hot in the barrel for too long gives yellowing that you cannot see until the bottle is next to a white one. Short stops are worse than long ones for this reason — a machine left idle at temperature for twenty minutes should be purged before it runs again.

Quality

Tests that decide acceptance

TestWhat it provesWhere it typically fails
Visual grading against a limit sampleSeam, flow lines, specks and haze are within what the brand acceptsSeam under the shoulder; base edge
Base thickness by sectionThe heavy base is where the drawing says, without bubblesBase centre; the gate mark
Pump fit and pull-off forceThe pump seats at the right height and does not pull outNeck squareness and bore diameter
Drop, filledThe bottle survives a bathroom-floor dropBase corner
Weight by cavityThe four or eight cavities are running the same wallOuter cavities on a wide die-head spacing
Annealing check after 24 hNo stress cracking at the baseBase corner where the wall changes fastest

Troubleshooting

Defects and where they come from

What you seeUsual causeWhat to change first
Haze through the bodyMoisture in the resin, or a cold die headCheck the dryer dew point, then raise the head temperature 5 °C
Bubbles in the baseWet resin, or the base insert too hot to freeze the meltDry the resin; drop the base circuit 3 – 4 °C
Visible seam on the shoulderPinch land worn, or blow pressure too highResurface the land; reduce pressure to 0.5 MPa
Yellow tint after a stopResin dwelled hot in the barrelPurge before restart; shorten the stop
Pump sits crookedNeck not square, or the insert is wornCheck insert squareness with a gauge, replace if worn
One cavity heavier than the othersDie-head spacing too wide for the parison, or uneven coolingCheck the profile per head, balance the circuits

Line

Line configuration and a worked example

ItemSpecification for a 100 ml PETG line
Blow molding machineKSY55-J2.5L, PETG screw and die head, two die heads, double station
Resin dryerDehumidifying dryer, 65 – 70 °C, dew point −20 °C
MouldTwo cavities, polished cavity, beryllium-copper base insert on its own circuit
De-flashingCut against the mould; a hand-trimmed seam shows on a clear bottle
PackingBagging at the machine; clear bottles scratch, so no bulk bin
ChillerAir-cooled, sized for the base circuit plus the body

Worked example: a 100 ml PETG bottle at 40 g, four cavities, 32 s cycle. Shot weight is 4 × 0.04 = 0.16 kg, so the plasticising demand is 0.16 ÷ 32 s = 18 kg/h, inside the 48 kg/h of the KSY55-J2.5L. Output is 3,600 ÷ 32 × 4 = 450 bottles an hour.

Shorten it to 24 s and the arithmetic gives 600 an hour, but the base has not frozen: the bottles come out with a soft centre that sinks as it cools, and the defect only shows up after the bottle has been standing for an hour. On a thick-base container the cycle is set by the base, not by the body.

Evidence

From projects we have built

A PETG thick-wall project in Indonesia runs a single die head with a dedicated PETG screw and a separately cooled base insert. The notes cover why the cycle has to be slow and what a cold base insert does to the clarity of the base. PETG thick-wall bottles: single head, controlled base.

For the material behaviour behind these settings see PETG thick-wall bottles, and for the container families the case studies index.

FAQ

Questions

PETG, PP or acrylic for a cosmetic bottle?

PETG for glass-like clarity and a heavy base. Clarified PP for a translucent bottle at lower cost and a wider process window. Acrylic is used for premium caps and thick-wall jars, not usually for the bottle body.

Why does PETG need drying?

PETG is hygroscopic. Moisture left in the pellet hydrolyses in the barrel and shows up as haze, bubbles in the base and a weak weld line. A dehumidifying dryer at 65 – 70 °C is part of the line, not an accessory.

How thick can the base be?

2 – 3 mm is normal for a cosmetic bottle, and the base is what sets the cycle: it is the last part to freeze. A separate cooling circuit in a beryllium-copper base insert is what makes a 30-second cycle possible on a thick base.

Why is the cycle longer than a shampoo bottle of the same size?

Because of the base. A 2.5 mm base needs three to four times the cooling of a 0.9 mm body, and no amount of blow pressure shortens it. Thick-wall containers are slow by design.

Can you hold the pump height?

Yes, if the neck insert is square and the blow pin concentric. Pump height is a neck dimension, not a machine setting; a 0.2 mm out-of-square neck leaks at the collar on the filling line.

How are cosmetic bottles inspected?

Against a limit sample: seam visibility, flow lines, specks, haze and base clarity, graded to an AQL the brand sets. It is a visual standard, which is why the light in the inspection area matters as much as the machine.

Can one machine make both clear and opaque bottles?

Only with a full material change: different screw, different temperatures and a thorough purge. In practice most plants dedicate a machine to PETG and run PP or HDPE on another.

Do you supply the mould and the base insert?

Yes. The base insert is specified separately because its material and cooling decide both the clarity of the base and the cycle time.

Get a quote

Send us your container

Send the drawing or a photo with volume, weight and material, and the output you need. We recommend the machine and mold.